Ceramic anti-corrosion and wear-resistant coating
Ceramic anti-corrosion and wear-resistant coating repair process: 1) Surface treatment and roughening (remove dust, dirt, oil, grease and other attachments on the metal surface to reveal the metallic luster. If there is no sandblasting equipment, the surface can be roughened by grinding to strengthen the repair material and metal adsorption capacity) 2) Mix components A and B evenly (the wear-resistant ceramic coating repair material is a two-component product, according to the weight ratio A:B=2:1; fully mix with a spatula, the mixing time is 3-5 minutes .At room temperature, the mixed material must be used up within 25 minutes, otherwise the material will become hard, which is not conducive to operation) 3) Coating construction (In order to facilitate smoothing the surface, use a hot tool spatula to scrape the mixed small particles of silicon carbide onto the surface to be repaired and protected. When it is semi-cured, pat the coating tightly and compact it, and iron it to level the picture. layer surface.)
隐藏域元素占位
Silicon carbide metal repair agent
Silicon carbide metal repair agent repair process: 1) Surface treatment and roughening (remove dust, dirt, oil, grease and other attachments on the metal surface to reveal the metallic luster. If there is no sandblasting equipment, the surface can be roughened by grinding to strengthen the repair material and metal adsorption capacity) 2) Prepare components A and B evenly (silicon carbide metal repair material is a two-component product, according to the weight ratio A:B=1:1; fully mix with a spatula, and the mixing time is 3-5 minutes. Room temperature Next, the mixed material must be used up within 25 minutes, otherwise the material will become hard, which is not conducive to operation) 3) Coating construction (In order to facilitate smoothing the surface, use a hot tool spatula to scrape the mixed small particles of silicon carbide onto the surface to be repaired and protected. When it is semi-cured, pat the coating tightly and compact it, and iron it to level the picture. layer surface.)
隐藏域元素占位
Wear-resistant ceramic particle glue
Wear-resistant ceramic particle glue repair process: 1) Surface treatment and roughening (remove dust, dirt, oil, grease and other attachments on the metal surface to reveal the metallic luster. If there is no sandblasting equipment, the surface can be roughened by grinding to strengthen the repair material and metal adsorption capacity) 2) Prepare components A and B evenly (the ceramic particle ball repair material is a two-component product, according to the weight ratio A:B=1:1; fully mix with a spatula, and the mixing time is 3-5 minutes. Room temperature Next, the mixed material must be used up within 25 minutes, otherwise the material will become hard, which is not conducive to operation) 3) Coating construction (In order to facilitate smoothing the surface, use a hot tool spatula to scrape the mixed small particles of silicon carbide onto the surface to be repaired and protected. When it is semi-cured, pat the coating tightly and compact it, and iron it to level the picture. layer surface.)
隐藏域元素占位
Pump casing impeller repair material
Pump casing impeller repair material repair process: 1) Surface treatment and roughening (remove dust, dirt, oil, grease and other attachments on the metal surface to reveal the metallic luster. If there is no sandblasting equipment, the surface can be roughened by grinding to strengthen the repair material and metal adsorption capacity) 2) Mix components A and B evenly (the wear-resistant ceramic coating repair material is a two-component product, according to the weight ratio A:B=1:1; fully mix with a spatula, the mixing time is 3-5 minutes .At room temperature, the mixed material must be used up within 25 minutes, otherwise the material will become hard, which is not conducive to operation) 3) Coating construction (In order to facilitate smoothing the surface, use a hot tool spatula to scrape the mixed small particles of silicon carbide onto the surface to be repaired and protected. When it is semi-cured, pat the coating tightly and compact it, and iron it to level the picture. layer surface.)
隐藏域元素占位
Wear-resistant ceramic protective agent
Wear-resistant ceramic particle glue repair process: 1) Surface treatment and roughening (remove dust, dirt, oil, grease and other attachments on the metal surface to reveal the metallic luster. If there is no sandblasting equipment, the surface can be roughened by grinding to strengthen the repair material and metal adsorption capacity) 2) Prepare components A and B evenly (the ceramic particle ball repair material is a two-component product, according to the weight ratio A:B=1:1; fully mix with a spatula, and the mixing time is 3-5 minutes. Room temperature Next, the mixed material must be used up within 25 minutes, otherwise the material will become hard, which is not conducive to operation) 3) Coating construction (In order to facilitate smoothing the surface, use a hot tool spatula to scrape the mixed small particles of silicon carbide onto the surface to be repaired and protected. When it is semi-cured, pat the coating tightly and compact it, and iron it to level the picture. layer surface.)
隐藏域元素占位
NEWS
undefined
Email:sdlijin2022@163.com
Address:No. 5111, Kuiwen District, Weifang City, Shandong Province, China
Tel:+86-536-7242727
Phone:+86-188-6636-7765
Website:www.sdlijin.com
Copyright © 2022 Shandong Lijin New Material Technology Co., Ltd.